抄録(英) This paper presents the molten bridge behaviors of Au-plated material at super low breaking velocity conditions by introducing our new designed test rig. The typical waveforms in the contact voltage and contact force during breaking were investigated under the load 5-25V/0.2-0.5A and velocity of 25-50nm/s. From the repetitive experimental results, we found that the intermittent molten bridge phenomena are formed from the competition of multitude contact a-spots for current distribution. Also, the possible bridge diameter is calculated with different bridge length and input power by using FEM thermal simulation and ISHIDA's experiment results. Finally, the effect of breaking velocity and electric load on bridge length and duration is also analyzed.
キーワード(和)
キーワード(英) molten bridge / contact a-spot / breaking velocity / thermal simulation
資料番号 EMD2014-71
発行日

研究会情報
研究会 EMD
開催期間 2014/11/22(から1日開催)
開催地(和)
開催地(英)
テーマ(和)
テーマ(英)
委員長氏名(和)
委員長氏名(英)
副委員長氏名(和)
副委員長氏名(英)
幹事氏名(和)
幹事氏名(英)
幹事補佐氏名(和)
幹事補佐氏名(英)

講演論文情報詳細
申込み研究会 Electromechanical Devices (EMD)
本文の言語 ENG
タイトル(和)
サブタイトル(和)
タイトル(英) Formation process of intermittent molten bridge between Au-plated contacts at super low breaking velocity
サブタイトル(和)
キーワード(1)(和/英) / molten bridge
第 1 著者 氏名(和/英) / Wanbin Ren
第 1 著者 所属(和/英)
School of Electrical Engineering and Automation, Harbin Inst. of Tech.
発表年月日 2014-11-29
資料番号 EMD2014-71
巻番号(vol) vol.114
号番号(no) 342
ページ範囲 pp.-
ページ数 6
発行日